Send Message
Home > products > Geomembrane Pond Liner >
0.3mm/0.5mm/0.75mm/1mm/1.5mm/2mm Black Membrane Plastic Sheet HDPE LDPE LLDPE Virgin Geomembrane Liner For Shrimp Fish F

0.3mm/0.5mm/0.75mm/1mm/1.5mm/2mm Black Membrane Plastic Sheet HDPE LDPE LLDPE Virgin Geomembrane Liner For Shrimp Fish F

2mm Black Membrane Plastic Sheet

1.5mm Black Membrane Plastic Sheet

0.75mm Black Membrane Plastic Sheet

Place of Origin:

China

Brand Name:

OEM

Certification:

ISO9001

Contact Us

Request A Quote
Product Details
Model NO.:
Hdpe Geomembrane
Description:
Shrimp Fish Farm Pond Dam Building Geomembrane Pond Liner
Raw Material:
HDPE LDPE LLDPE
Width:
1m-8m
Another Name:
HDPE Geomembrane Waterproof Liner
Usage:
Waterproof Projects
Product Description
HDPE Geomembrane Technical Parameter (GB standard)
Spec
Properties
GMS0.5
GMS0.75
GMS1.0
GMS1.25
GMS1.5
GMS2.0
GMS2.5
Thickness
0.5mm
0.75mm
1.0mm
1.25mm
1.5mm
2.0mm
2.5mm
Tensile Properties
(each direction) (≥)
.yield strength
.break strength
.yield elongation
.break elongation


7KN/m
10KN/m
--
600%


10KN/m
15KN/m
--
600%


13KN/m
20KN/m
11%
600%


16KN/m
25KN/m
11%
600%


20KN/m
30KN/m
11%
600%


26KN/m
40KN/m
11%
600%


33KN/m
50KN/m
11%
600%
Density(≥)
0.940g/cc
0.940g/cc
0.940g/cc
0.940g/cc
0.940g/cc
0.940g/cc
0.940g/cc
Puncture Restistance (≥)
120N
180N
240N
300N
360N
480N
600N
Carbon Black Content
2.0-3.0%
2.0-3.0%
2.0-3.0%
2.0-3.0%
2.0-3.0%
2.0-3.0%
2.0-3.0%
Carbon black Dispersion
Noted(1)
Noted(1)
Noted(1)
Noted(1)
Noted(1)
Noted(1)
Noted(1)
Tear Resistance (≥)
56N
84N
115N
140N
170N
2255N
280N
Oxidative Induction Time(OIT)
Standare OIT(≥)

60min.

60min.

60min.

60min.

60min.

60min.
60min.

Basic Details
Geomembrane; pond liner
1.Main Thickness:0.1mm,0.2mm,0.3mm,0.5mm, 0.75mm,1.0mm,1.5mm,2.0mm,3.0mm,4.0mm,5.0mm
2.Main Width:4m, 5m, 5.8m, 6.0m, 7m, 8m,10m
3.Main Length:50m/100m
4.Main Color: black, white, blue, green
5. Optional surface: Textured or Smooth surface.
6.Material:HDPE, LDPE,LLDPE,EVA
7. Certificate & Test: ISO, TUV,SGS
8. Quality Control: Third party test and factory lab test

 

The polyethylene geomembrane is made of high-quality polyethylene virgin resin,the main component is 97.5% polyethylene,2.5% carbon black,anti-aging agent,antioxidant,ultraviolet absorber,stabilizer and other additives, using internationally advanced mutiple layer co-extrusion blow molding process or muti-head flat extrusion process.The finished product has excellent resistance to chemical acid and alkali,UV resistance, strength, durability and stress tear resistance.

0.3mm/0.5mm/0.75mm/1mm/1.5mm/2mm Black Membrane Plastic Sheet HDPE LDPE LLDPE Virgin Geomembrane Liner For Shrimp Fish F 0

HDPE Geomembrane Application:
(1)Aquaculture:
Using the geomembrane anti-seepage feature; geomembrane liners can be used as fish ponds, shrimp pond, tank liner and others.

(2)Landfill:
HDPE geomembrane is the most widely used in landfill anti-seepage engineering material. The use of main parts of the bottom of the landfill liner, landfill sealing cover, leachate regulating pool liner, etc.

(3)Water Treatment System :
HDPE geomembrane is applied to the adjustment of the power plant and sewage treatment plants pool;and a series of water treatment systems.
(4
)Agriculture:
HDPE geomembrane suitable
Agriculture: washing pool, pool heap leaching, heap yard, dissolving tank, tank, storage area, the bottom line of the tailings seepage control, etc

0.3mm/0.5mm/0.75mm/1mm/1.5mm/2mm Black Membrane Plastic Sheet HDPE LDPE LLDPE Virgin Geomembrane Liner For Shrimp Fish F 1

0.3mm/0.5mm/0.75mm/1mm/1.5mm/2mm Black Membrane Plastic Sheet HDPE LDPE LLDPE Virgin Geomembrane Liner For Shrimp Fish F 2

 Construction Method

1. The slope shall be laid in order from top to bottom. Don't pull it too tight.
2. Tow adjacent longitudinal joints should not be in a horizontal line, should bestaggered more than 1m each other.
3. Longitudinal joints should be more than 1.50m away from the dam foot and bending foot, and should be located on the plane.
4. When the slope is laid, the direction of spreading film should be basically parallel to the slope line.
5. The construction, first of all to use small diameter sand or clay levelingbase, and then laid the geomembrane. The geomembrane should not be stretched too tight, and the part of the soil bured at both ends is corrugated. A transitional layer of about 10cm is laid on the geomembrane with sand or clay.
 

FAQ

1.Are you manufacturer or trade company?
We Zhonglu are a professional geosynthetic products manufacture, we will provide you with top-class service.

2. What's the order process?
a.Inquiry--- The more detailed information you provide, the more accurate product we could provide you.
b. Quotation---Resonable quotation with clear specifications.
c. Sample confirmation---Sample could be sent before the final ordering.
d. T/T 30% in advanced, and the balance could be paid before shipment.
e. Production---Mass production.
f. Shipping--- By sea, air or courier. Detailed picture of package could be provided.

3. How long is your delivery time?
Generally it is 3-5 days if the goods are in stock. or it is 5-7 days if the goods are not in stock, it is according to quantity.

4. How does your factory do regarding quality control?
"Quality is priority." We always attach great importance to quality controlling from the beginning to the end.

5.What's the payment method you accept?
T/T, L/C,D/P etc.




Professional geosynthetics manufacturer
Anhui Zhonglu Engineer Materials Co., Ltd
Angela:86-18095658976

 

Send your inquiry directly to us

Privacy Policy China Good Quality Geotextile Geogrid Supplier. Copyright © 2023-2024 geotextilegrid.com . All Rights Reserved.